Material problems that can occur in 4mm2 solar cables

18, Apr. 2024

PVC plastic: many impurities, unqualified thermal weight loss, pores in the extruded layer, difficult to plasticize, incorrect color, etc.

 

PVC plastic: many impurities, unqualified thermal weight loss, pores in the extruded layer, difficult to plasticize, incorrect color, etc.
 
  PVC tape: too thick, insufficient tension, short ends, uneven thickness, etc.
 
  PE filled rubber strip: a little hard, easy to break, and the curvature is not equal.
 

Copper tape: uneven thickness, oxidation and discoloration, insufficient tension, wrinkles, insufficient softening, hard, short sides, poor connection, peeling paint film or zinc layer, etc.
 
Copper rod: It is made of recycled miscellaneous copper, the surface is oxidized and discolored, the tension is insufficient, and it is not round.
 
    XLPE insulation material: short scorch resistance time, easy to crosslink in the early stage, etc.
 
  Silane cross-linked materials: poor extrusion temperature control, low thermal elongation, rough surface, etc.
 
  Halogen-free rubber coated flame retardant tape: easy to break, wrinkles on the reel, threading, poor flame retardancy, smoke, etc.

For more Advantage of Electric Motor, Slip Definition in Motor, What Are Slip Ringsinformation, please contact us. We will provide professional answers.